Description
Heavy
Oxidation $ Scratch Repair
Utilized in
a multi-step procedure on clad, cast or forged aluminum, nickel, stainless
steel, etc.
Application:
1. Apply
sparingly. Polish with tufted wool compounding pad on a circular buffer
(1600-2000 rpm).
2. Polish
until oxidation and residue disappear, about 60 seconds.
3. Repeat
if oxidation cloudiness remains. Badly deteriorated surfaces may call for
NUSHINE IIF9.
4. Final
finish with NUSHINE IIS.
Not
recommended for clear coated finishes.
Test References:
·
AMS1650
·
D6-17487
·
CSD1
Packing
Sizes:
1/4lb., 1/2lb.,
1lb., 10lb., 50lb.